REGENERASI KATALIS Mg/Al-HIDROTALSIT PADA SINTESIS BIODIESEL BERBAHAN BAKU MINYAK BIJI KAPUK
Abstrak (Bhs. Indonesia)
Telah dilakukan sintesis Mg/Al-hidrotalsit sebagai katalis pembuatan biodiesel dari minyak biji kapuk. Mg/Al-hidrotalsit disintesis menggunakan metode kopresipitasi. Mg/Al-hidrotalsit yang telah digunakan dalam pembuatan biodiesel kemudian diregenerasi menggunakan metode kalsinasi. Mg/Al-hidrotalsit hasil sintesis dikarakterisasi dengan XRD, FTIR dan BET. Hasil XRD menunjukkan Mg/Al-hidrotalsit telah terbentuk. Spektra FTIR menunjukan terbentuknya Mg/Al-hidrotalsit dengan interlayer CO32-. Mg/Al-hidrotalsit setelah diregenerasi dikarakterisasi menggunakan FTIR dan BET. Spektra FTIR menunjukkan Mg/Al-hidrotalsit setelah diregenerasi mengalami pengurangan CO32- ditandai dengan hilangnya uluran asimetris O=C-O pada bilangan gelombang 1482,06 cm-1. Mg/Al-hidrotalsit hasil sintesis memiliki luas permukaan 7,665 m2; rerata jejari pori 27,382 Å dan volume pori total 86,7308 e-03 cc/g. Mg/Al-hidrotalsit setelah diregenerasi mengalami kenaikan luas permukaan menjadi 12,873 m2, rerata jejari pori meningkat menjadi 37,961 Å dan volume pori mengalami kenaikan menjadi 94,7242 e-03 cc/g. Konversi biodiesel yang dihasilkan sebesar 60,43%.
Abtrak (Bhs. Inggris)
Mg/Al-hydrotalcites synthesis as a catalyst catalyst for producing biodiesel from cottonseed oil had been done by co-precipitation method. Mg/Al-hydrotalcites have been used to produce biodiesel then regenerated by calcination method. Synthesized Mg/Al-hydrotalcites was characterized by XRD, FTIR and BET. The XRD result showed that Mg/Al-hydrotalcites has been formed. The FTIR spectra showed that the Mg/Al-hydrotalcites was formed by the appearance of CO32- interlayer. The Mg/Al-hydrotalcites after regeneration treatment was characterized by FTIR and BET. The FTIR spectra showed that Mg/Al-hydrotalcites after regenerated, experienced a decrease CO32- characterized by loss of stretching asymmetrical O=C-O on the waves number 1482,06 cm-1. Synthesized Mg/Al-hydrotalcites compound had surface area 7,665 m2; average pores radius 27,382 Å; and total pores volume 86,7308 e-03 cc/g. After regenerated, Mg/Al-hydrotalcites experienced an increased the surface area to 12,873 m2, increased the average pores radius to 37,961 Å and increased the total pores volume to 94,7242 e-03 cc/g. Conversion of biodiesel produced equal to 60,43%.
Kata kunci
Pembimbing 1
Pembimbing 2
Pembimbing 3
Tahun
Jumlah Halaman
Save